Pavers are a driveway with extra failure modes. The surface can take a wash. The joints are sand, polymeric sand, or moss, and a pressure washer treats all three as something to excavate if you let it. Sealer is a second project that this site does not sell. Cleaning well and sealing too soon is how a patio turns cloudy.
The flatwork method is the driveway how-to. The attachment is how to use a surface cleaner. The machine class is the driveway washer guide. If the “pavers” are a wood deck, you are on the wrong page. Use the deck guide.
Look at the joints before you look at the PSI
Concrete pavers, clay brick, and wet-cast stone do not behave the same, and this page will not pretend one pressure number fits all three. What they share is a joint. Loose sand washes out. Polymeric sand, once it has cured, resists a gentle rinse and still fails if you park a 0-degree tip in the crack. Moss in a joint is often what people wanted gone, and it is also what was keeping the joint full.
Walk the patio. If the sand is new, stop and get the cure time from whoever installed it. Washing polymeric sand on day two is how you buy another bag and another weekend. If the joints are already half empty, plan to re-sand after the wash. Do not seal first in the hope the sealer will glue the dirt down. It will.
Weeds in the joints come out better with a knife or a flame the local rules allow than with a cutting tip. The tip removes the weed and the sand under it.
Note the sealer, if there is one. A film that beads water is existing sealer. Pressure washing can haze it, strip it in patches, or leave it alone. You will not know from across the yard. Test a corner you can live with. If the sealer is peeling, you may need a stripper the sealer maker names. That product is not in this catalog.
Chemical, then water
Sweep the grit off. Sand on the surface becomes a blast medium. Move furniture. Wet plants.
Oil and tire film on a paver drive are the same stains as on a slab. The Krud Kutter Concrete and Driveway concentrate, model 385466, is bleach-free on its listing, makes up to 20 gallons on that page, and should sit 3 to 5 minutes without drying. An older sheet for a different driveway concentrate used a different dwell. Read the jug that matches 385466. The listing is a concrete and driveway product. If your pavers are something that jug does not name, do not stretch it. The soap guide is the rest of the shelf.
The 30 SECONDS Outdoor Cleaner names concrete among other outdoor surfaces and says mix 1:1. It does not, in the text we checked, say to run it through the pump. Organic slime on a shaded patio is the stain people buy it for. Keep it out of the washer unless the bottle you are holding says otherwise. Do not mix it with the Krud Kutter jug, with ammonia, or with acids.
Apply, dwell, and do not let the mix dry in the sun. Pavers get hot. A cloudy morning is easier than a July afternoon.
The rinse that leaves the sand
Use a surface cleaner sized to the washer, flat on the pavers, in overlapping passes. The Simpson 80165 manual ceiling is 3.0 GPM and 3,700 PSI. The Westinghouse WPX3400 at 2.6 GPM and 3,400 PSI is inside that. The PWSC12 is the 12-inch electric deck, not a gas deck. The full pairing is in the surface cleaner guide. Do not lift the shroud while the bar is spinning. A tipped deck will dig a joint in one pass.
Edges and steps go to a fan tip on the wand. White or green, from the nozzle guide. Yellow, 15 degrees, only if you are moving and the joint is not in the middle of the fan. Red, 0 degrees, is how a patio loses its sand in straight lines. There is no paver job on this page that starts with red.
A small electric will wash a landing. The Greenworks GPW2300 is 1.2 GPM rated, with a 2.3 GPM maximum at low pressure in the Greenworks description. A large patio is the gas class: WPX3400, Simpson PS3228 at 2.5 GPM, or the BE B2565HGS at 3.0 GPM and 2,500 PSI. None of those is a test we ran on pavers. They are the published flows.
If the wash is pulling sand out, stop. Back up, open the fan, or switch to the surface cleaner and a slower pace. You can always re-sand. You cannot un-etch a face you stood on with a turbo nozzle. Some electric listings include a turbo tip. Leave it in the box for pavers.
Rinse plants. Flush soap out of the washer if you used the tank. Let the patio dry until the color stops changing. Wet pavers look clean and are still full of water.
Sand, if the joints need it
This site does not list polymeric sand or a joint stabilizer. Buy what the paver maker specifies. Ordinary sand and polymeric sand are not interchangeable, and polymeric products have their own water-and-cure steps that you should take from that bag, not from this article.
Sweep sand into joints that are actually empty. Do not bury the face of the paver. If the product needs a light mist to set, mist. Do not return with the surface cleaner the same day to “knock the haze off.” That is how the new sand leaves.
Wait out the cure the bag names before anyone parks a car on it or you start thinking about sealer.
Sealer, from someone else’s label
There is no sealer in src/data/products.json, so there is no Check price button for one. That is deliberate. A sealer matched to the wrong paver, or laid over a sealer that needed stripping, clouds, peels, or stays sticky. The maker of the paver, or the label of the sealer already on them, is the source.
What this page will say, because it is true of water-based and solvent sealers alike: the pavers have to be dry to the standard that label sets. A sunny hour is not a moisture meter. Trapped water is the white haze people blame on “cheap sealer” when the surface was simply damp. Temperature and rain forecasts are on the label for the same reason.
Test one paver or a corner. Color-enhancing sealers darken the stone. If you wanted the washed color, an enhancing sealer is the wrong can. Film-forming sealers can be slippery when wet. That is a patio safety question, not a gloss question. Read it before you coat the only walk to the door.
If old sealer is peeling, stripping is its own chemical job. Do not pressure wash peeling sealer into the grass and then coat over the flakes that stayed. You will see every flake forever.
Apply sealer the way the can says, usually a thin coat, and do not walk on it early because a footprint felt inevitable. Two thin coats, if the label allows a second, beat one heavy coat that puddles in the joints.
What a clean patio is allowed to look like
Oil can ghost. Efflorescence, the white mineral film some pavers push out, is not dirt and may return after a wash. Moss in a permanent shade will return. None of that means the washer was too small.
Look down the rows in low sun. Wand stripes show on pavers the same way they show on a slab. One more overlapping pass with the surface cleaner, after the chemical has done its work, is the fix. A larger PSI number is not.
If you are washing someone else’s patio for money, the side business guide applies: say what will lighten rather than vanish, and do not quote a price from a video. Sealing is a separate line on the quote because it is a separate dry time. Do not fold it into the wash and hope the weather cooperates by evening.